{"id":6204,"date":"2022-11-21T19:38:35","date_gmt":"2022-11-22T03:38:35","guid":{"rendered":"https:\/\/zetarmoulding.com\/?p=6204"},"modified":"2022-11-21T21:44:04","modified_gmt":"2022-11-22T05:44:04","slug":"formulation-design-of-heat-resistant-rubber","status":"publish","type":"post","link":"https:\/\/zetarmoulding.com\/tr\/isiya-dayanikli-kaucuk-formulasyon-tasarimi\/","title":{"rendered":"Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk form\u00fclasyon tasar\u0131m\u0131"},"content":{"rendered":"<p><strong>Is\u0131n\u0131n kau\u00e7uk \u00fcr\u00fcnlere zarar verebilece\u011fi bir s\u0131r de\u011fildir. Ancak kau\u00e7u\u011fu y\u00fcksek s\u0131cakl\u0131klara dayanabilecek \u015fekilde form\u00fcle etmenin yollar\u0131 oldu\u011funu biliyor muydunuz? <\/strong><\/p>\n\n\n\n<p><strong>Bu blog yaz\u0131s\u0131nda, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7u\u011fu form\u00fcle etmenin farkl\u0131 yollar\u0131n\u0131 ve bunlar\u0131n i\u015finize nas\u0131l fayda sa\u011flayabilece\u011fini inceleyece\u011fiz. Ayr\u0131ca bir form\u00fclasyon y\u00f6ntemi se\u00e7erken g\u00f6z \u00f6n\u00fcnde bulundurman\u0131z gereken baz\u0131 fakt\u00f6rleri de tart\u0131\u015faca\u011f\u0131z. Kau\u00e7uk \u00fcr\u00fcnlerinizi \u0131s\u0131dan koruman\u0131n bir yolunu ar\u0131yorsan\u0131z, okumaya devam edin!<\/strong><\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"375\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-1.jpg\" alt=\"\" class=\"wp-image-6220\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-1.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-1-300x199.jpg 300w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<h2 class=\"wp-block-heading\"><mark style=\"background-color:rgba(0, 0, 0, 0)\" class=\"has-inline-color has-vivid-cyan-blue-color\">Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk nedir ve neden buna ihtiyac\u0131m\u0131z var?<\/mark><\/h2>\n\n\n\n<p>Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk, y\u00fcksek s\u0131cakl\u0131klara dayanacak \u015fekilde tasarlanm\u0131\u015f elastik bir malzemedir. Conta, ke\u00e7e ve hortum gibi \u00e7e\u015fitli end\u00fcstriyel ve ticari uygulamalarda yayg\u0131n olarak kullan\u0131l\u0131r. <\/p>\n\n\n\n<p><a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk <\/a>di\u011fer malzeme t\u00fcrlerine g\u00f6re bir\u00e7ok avantaja sahiptir. Dayan\u0131kl\u0131d\u0131r, esnektir ve m\u00fckemmel \u0131s\u0131 direncine sahiptir. <\/p>\n\n\n\n<p>Ayr\u0131ca, <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">\u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk <\/a>genellikle di\u011fer se\u00e7eneklerden daha uygun maliyetlidir. Ad\u0131ndan da anla\u015f\u0131laca\u011f\u0131 gibi, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk, y\u00fcksek s\u0131cakl\u0131klara diren\u00e7 gerektiren uygulamalar i\u00e7in ideal bir malzemedir. <\/p>\n\n\n\n<p>Bununla birlikte, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7u\u011fun \u0131s\u0131 hasar\u0131na kar\u015f\u0131 tamamen ba\u011f\u0131\u015f\u0131k olmad\u0131\u011f\u0131 unutulmamal\u0131d\u0131r. Uzun s\u00fcre \u0131s\u0131ya maruz kald\u0131\u011f\u0131nda eninde sonunda bozunacakt\u0131r. Buna ra\u011fmen, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uklar bir\u00e7ok uygulamada m\u00fckemmel performans sa\u011flar.<\/p>\n\n\n\n<p>Is\u0131 direnci, kau\u00e7uk ve \u00fcr\u00fcnlerinin uzun s\u00fcreli termal ya\u015flanmaya maruz kald\u0131ktan sonra fiziksel ve mekanik \u00f6zelliklerini veya performans\u0131n\u0131 koruma kabiliyetini ifade eder. Esasen bu nitelikte bir d\u00fc\u015f\u00fc\u015f yoktur. <\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"344\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-2.jpg\" alt=\"\" class=\"wp-image-6222\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-2.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-2-300x183.jpg 300w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<p>Y\u00fcksek s\u0131cakl\u0131ktaki fiziksel ve mekanik \u00f6zellikler ile oda s\u0131cakl\u0131\u011f\u0131ndaki \u00f6zellikler aras\u0131ndaki fark k\u00fc\u00e7\u00fckt\u00fcr, yani s\u0131cakl\u0131k direnci iyidir. Kau\u00e7u\u011fun fiziksel ve mekanik \u00f6zelliklerinin (test) s\u0131cakl\u0131\u011f\u0131 ile de\u011fi\u015fimini g\u00f6sterir. <\/p>\n\n\n\n<p><a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">(Is\u0131ya dayan\u0131kl\u0131) kau\u00e7uk \u00fcr\u00fcnler<\/a> y\u00fcksek s\u0131cakl\u0131klarda kullan\u0131ld\u0131\u011f\u0131nda iyi \u0131s\u0131 direncine ve iyi s\u0131cakl\u0131k direncine sahip olmal\u0131d\u0131r. <\/p>\n\n\n\n<p>Is\u0131 direncini de\u011ferlendirmek i\u00e7in Martin \u0131s\u0131 direnci ve Vicat \u0131s\u0131 direncini kullanmak gibi bir\u00e7ok yol vard\u0131r.<\/p>\n\n\n\n<p>Ayr\u0131\u015fma s\u0131cakl\u0131\u011f\u0131, malzemenin servis s\u0131cakl\u0131\u011f\u0131n\u0131n \u00fcst s\u0131n\u0131r\u0131 olarak termogravimetrik alet arac\u0131l\u0131\u011f\u0131yla veya k\u00fctlenin 50% (Tn) kadar azald\u0131\u011f\u0131 s\u0131cakl\u0131k olan 40 ila 45 dakika boyunca vakumlu \u0131s\u0131tma yoluyla da bulunabilir - \u0131s\u0131 direncini de\u011ferlendirmek i\u00e7in yar\u0131 \u00f6m\u00fcr s\u0131cakl\u0131\u011f\u0131.<\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"375\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-3.jpg\" alt=\"\" class=\"wp-image-6223\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-3.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-3-300x199.jpg 300w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<p>Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk, y\u00fcksek s\u0131cakl\u0131k ko\u015fullar\u0131 alt\u0131nda orijinal mekanik \u00f6zelliklerini ve kullan\u0131m de\u011ferini uzun s\u00fcre koruyabilen vulkanize kau\u00e7u\u011fu ifade eder. <\/p>\n\n\n\n<p>\u00d6zelliklerdeki de\u011fi\u015fim miktar\u0131 (sertlik gibi) ve \u00f6zelliklerdeki de\u011fi\u015fim oran\u0131 (\u00e7ekme mukavemeti gibi), performans tutma oran\u0131 ve ya\u015flanma katsay\u0131s\u0131, mekanik \u00f6zelliklerinin de\u011fi\u015fimini g\u00f6sterir. <\/p>\n\n\n\n<p>Kau\u00e7uk s\u0131zd\u0131rmazl\u0131k \u00fcr\u00fcnlerinde, vulkanize kau\u00e7u\u011fun s\u0131k\u0131\u015ft\u0131r\u0131lm\u0131\u015f durumdaki \u0131s\u0131 direncine \u0131s\u0131 direnci s\u0131k\u0131\u015ft\u0131rma performans\u0131 denir ve bu genellikle s\u0131k\u0131\u015ft\u0131rma set katsay\u0131s\u0131 veya s\u0131k\u0131\u015ft\u0131rma gerilimi gev\u015feme katsay\u0131s\u0131 ile de\u011ferlendirilir.<\/p>\n\n\n\n<p>80\u00b0C'nin \u00fczerinde uzun s\u00fcreli kullan\u0131mdan sonra temel olarak orijinal performans\u0131n\u0131 ve kullan\u0131m de\u011ferini koruyabilen kau\u00e7uk \"\u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk\" kategorisine girer. Is\u0131ya dayan\u0131kl\u0131 ve y\u00fcksek s\u0131cakl\u0131k performans\u0131 <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">silikon kau\u00e7uk \u00fcr\u00fcnler<\/a> kau\u00e7u\u011fun \u00f6zel \u00f6zellikleri aras\u0131nda en yayg\u0131n performanst\u0131r. <\/p>\n\n\n\n<p>Bu durumda kau\u00e7u\u011fun istikrarl\u0131 performans\u0131n\u0131n temel nedeni, oksijen, ozon, a\u015f\u0131nd\u0131r\u0131c\u0131 kimyasallar, y\u00fcksek enerjili radyasyon ve y\u00fcksek s\u0131cakl\u0131klarda mekanik yorgunluk gibi fakt\u00f6rlerin etkisine direnebilmesidir. \u0130yi performans.<\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"564\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-4.jpg\" alt=\"\" class=\"wp-image-6224\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-4.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-4-300x300.jpg 300w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-4-150x150.jpg 150w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-4-100x100.jpg 100w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<h3 class=\"wp-block-heading\"><strong><mark style=\"background-color:rgba(0, 0, 0, 0)\" class=\"has-inline-color has-vivid-cyan-blue-color\">\u00c7al\u0131\u015fma s\u0131cakl\u0131\u011f\u0131 aral\u0131\u011f\u0131\/\u00b0C Uygulanabilir kau\u00e7uk<\/mark><\/strong><\/h3>\n\n\n\n<p>70\uff5e100 Do\u011fal kau\u00e7uk, stiren-b\u00fctadien kau\u00e7uk<\/p>\n\n\n\n<p>100\uff5e130 Neopren kau\u00e7uk, nitril kau\u00e7uk, epiklorohidrin kau\u00e7uk<\/p>\n\n\n\n<p>130\uff5e150 B\u00fctil kau\u00e7uk, etilen propilen kau\u00e7uk, kloros\u00fclfonlanm\u0131\u015f polietilen kau\u00e7uk<\/p>\n\n\n\n<p>150\uff5e180 Akrilik kau\u00e7uk, hidrojenlenmi\u015f nitril kau\u00e7uk<\/p>\n\n\n\n<p>180\uff5e200 vinil silikon kau\u00e7uk, flor kau\u00e7uk<\/p>\n\n\n\n<p>200\uff5e250 Dimetil silikon kau\u00e7uk, flor kau\u00e7uk<\/p>\n\n\n\n<p>\uff1e250 Perfloroeter kau\u00e7uk, florosilikon kau\u00e7uk, borosilikat kau\u00e7uk<\/p>\n\n\n\n<p><strong>Ulusal standart kau\u00e7u\u011fun s\u0131cakl\u0131k direnci a\u015fa\u011f\u0131daki iki dereceye ve be\u015f kategoriye ayr\u0131labilir<\/strong><\/p>\n\n\n\n<p>NR, IR, BR, 237 SBR, CR gibi s\u0131radan kau\u00e7uk A -70 \uff5e -30 \u2103 \/ 90 \uff5e 120 \u2103.<\/p>\n\n\n\n<p>NBR, IIR, EPDM, CSM gibi s\u0131radan kau\u00e7uk B -40\uff5e-20\u2103\/120\uff5e150\u2103.<\/p>\n\n\n\n<p>S\u0131radan kau\u00e7uk C -30 \uff5e 10 \u2103 \/ 80 \uff5e 90 \u2103, T, U gibi.<\/p>\n\n\n\n<p>ACM, ANM, EVA, CO, ECO gibi \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk A -30 \uff5e -10 \u2103 \/ 150 \uff5e 200 \u2103.<\/p>\n\n\n\n<p>MQ, MVQ, FPM, FKM gibi \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk B -70 \uff5e -20 \u2103 \/ 250 \uff5e 300 \u2103.<\/p>\n\n\n\n<p>Bununla birlikte, ger\u00e7ek kullan\u0131mda, \u00e7e\u015fitli i\u00e7 ve d\u0131\u015f fakt\u00f6rlerin etkisi nedeniyle, g\u00fcvenli bir hizmet \u00f6mr\u00fc sa\u011flamak i\u00e7in, genel dien kau\u00e7uk yakla\u015f\u0131k 100 \u00b0 C'de, ya\u011fa dayan\u0131kl\u0131 nitril kau\u00e7uk 130 \u00b0 C'de ve akrilat kau\u00e7uk 180 \u00b0 C'de kontrol edilir. \u2103. <\/p>\n\n\n\n<p>Silikon ve flor kau\u00e7u\u011fun s\u0131cakl\u0131\u011f\u0131 200-250\u00b0C'dir ve k\u0131sa s\u00fcreli kullan\u0131m i\u00e7in 300-350\u00b0C'ye ula\u015fabilir. Ayr\u0131ca 4 kategori vard\u0131r:<\/p>\n\n\n\n<p>Is\u0131 direnci <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">silikon kau\u00e7uk \u00fcr\u00fcnler<\/a> esas olarak kullan\u0131lan kau\u00e7u\u011fun t\u00fcr\u00fcne ba\u011fl\u0131d\u0131r. Bu nedenle form\u00fcl tasarlan\u0131rken \u00f6ncelikle ham kau\u00e7uk se\u00e7imi g\u00f6z \u00f6n\u00fcnde bulundurulmal\u0131d\u0131r.<\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"376\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/Silicone-Rubber-Products-31.jpg\" alt=\"\" class=\"wp-image-6116\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/Silicone-Rubber-Products-31.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/Silicone-Rubber-Products-31-300x200.jpg 300w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<p>Kau\u00e7u\u011fun \u0131s\u0131 direnci, y\u00fcksek viskoz ak\u0131\u015f s\u0131cakl\u0131\u011f\u0131, y\u00fcksek termal ayr\u0131\u015fma kararl\u0131l\u0131\u011f\u0131 ve kau\u00e7u\u011fun iyi termokimyasal kararl\u0131l\u0131\u011f\u0131 ile kendini g\u00f6sterir.<\/p>\n\n\n\n<p>Kau\u00e7u\u011fun viskoz ak\u0131\u015f s\u0131cakl\u0131\u011f\u0131, kau\u00e7u\u011fun molek\u00fcler yap\u0131s\u0131n\u0131n polaritesine ve molek\u00fcler zincirin sertli\u011fine ba\u011fl\u0131d\u0131r. Polarite ve sertlik ne kadar b\u00fcy\u00fckse viskoz ak\u0131\u015f s\u0131cakl\u0131\u011f\u0131 da o kadar y\u00fcksek olur. <\/p>\n\n\n\n<p>Kau\u00e7uk molek\u00fcllerinin polaritesi, polar gruplar\u0131 ve molek\u00fcler yap\u0131s\u0131 taraf\u0131ndan belirlenir ve molek\u00fcler zincirlerin sertli\u011fi de polar s\u00fcbstit\u00fcentlerin d\u00fczenlili\u011fi ve uzamsal yap\u0131 d\u00fczenlemeleri ile ilgilidir. <\/p>\n\n\n\n<p>Kau\u00e7uk molek\u00fcllerine 238 siyano grubu, ester grubu, hidroksil grubu veya klor atomu, flor atomu vb. eklenmesi \u0131s\u0131 direncini art\u0131racakt\u0131r. <\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"550\" height=\"550\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Products-1.jpg\" alt=\"\" class=\"wp-image-4661\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Products-1.jpg 550w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Products-1-300x300.jpg 300w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Products-1-150x150.jpg 150w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Products-1-100x100.jpg 100w\" sizes=\"auto, (max-width: 550px) 100vw, 550px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<p>Kau\u00e7u\u011fun termal ayr\u0131\u015fma s\u0131cakl\u0131\u011f\u0131, kau\u00e7u\u011fun molek\u00fcler yap\u0131s\u0131n\u0131n kimyasal ba\u011f \u00f6zelliklerine ba\u011fl\u0131d\u0131r. <\/p>\n\n\n\n<p>Kimyasal ba\u011f enerjisi ne kadar y\u00fcksek olursa, \u0131s\u0131 direnci de o kadar iyi olur. Borosilikat kau\u00e7uk gibi makromolek\u00fcler zincirler, <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">silikon kau\u00e7uk<\/a>ve polifenilsiloksan y\u00fcksek ba\u011f enerjisine sahiptir, bu nedenle m\u00fckemmel \u0131s\u0131 direncine sahiptirler.<\/p>\n\n\n\n<p>Genel olarak, flor i\u00e7eren FPM hari\u00e7, karbon zincirli kau\u00e7uk d\u00fc\u015f\u00fck \u0131s\u0131 direncine sahiptir ve 150-200\u00b0C s\u0131cakl\u0131kta uzun s\u00fcre kullan\u0131labilir; <\/p>\n\n\n\n<p>Ana zincir, Q tipi gibi elemental organik polimerler gibi hi\u00e7 karbon atomu i\u00e7ermez, Is\u0131 direnci \u00e7ok iyidir ve silika jel 250 \u00b0 C hatta 300 \u00b0 C'de uzun s\u00fcre kullan\u0131labilir.<\/p>\n\n\n\n<p>Kau\u00e7u\u011fun kimyasal stabilitesi \u0131s\u0131 direnci i\u00e7in \u00f6nemli bir fakt\u00f6rd\u00fcr, \u00e7\u00fcnk\u00fc y\u00fcksek s\u0131cakl\u0131k ko\u015fullar\u0131nda, baz\u0131 kimyasal maddeler oksijen, ozon, asit, alkali ve organik \u00e7\u00f6z\u00fcc\u00fclerle temas ederse.<\/p>\n\n\n\n<p>Kau\u00e7u\u011fun korozyonunu te\u015fvik edecek ve \u0131s\u0131 direncini azaltacakt\u0131r. Kimyasal stabilite kau\u00e7u\u011fun molek\u00fcler yap\u0131s\u0131 ile yak\u0131ndan ilgilidir. <\/p>\n\n\n\n<p>D\u00fc\u015f\u00fck doymam\u0131\u015fl\u0131\u011fa sahip b\u00fctil kau\u00e7uk, etilen-propilen kau\u00e7uk ve kloros\u00fclfonlanm\u0131\u015f polietilen m\u00fckemmel \u0131s\u0131 direnci g\u00f6sterir. <\/p>\n\n\n\n<p>Buna ek olarak, ana zincir \u00fczerinde tek bir ba\u011f ile ba\u011flanm\u0131\u015f aromatik bir yap\u0131 varsa, molek\u00fcler zincir de konjugasyon etkisi sayesinde yap\u0131y\u0131 stabilize edecektir.<\/p>\n\n\n\n<p>Bu <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">kau\u00e7u\u011fun \u0131s\u0131 direnci<\/a> kau\u00e7uk molek\u00fcler zincirinin doygunluk derecesi, molek\u00fcler zincirin sertli\u011fi, molek\u00fcl\u00fcn polaritesi ve kimyasal ba\u011f\u0131n do\u011fas\u0131 ile ilgilidir. A\u015fa\u011f\u0131daki molek\u00fcler yap\u0131ya sahip kau\u00e7uk daha iyi \u0131s\u0131 direncine sahiptir. <\/p>\n\n\n\n<p>Butil kau\u00e7uk, etilen propilen kau\u00e7uk vb. gibi molek\u00fcler zincir doygunlu\u011fu y\u00fcksektir; kau\u00e7uk ana zincir segmentinde daha fazla inorganik zincir vard\u0131r, \u00f6rne\u011fin <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">silikon kau\u00e7uk<\/a> bir silikon-oksijen yap\u0131s\u0131d\u0131r; <\/p>\n\n\n\n<p>Kau\u00e7uk molek\u00fcler zinciri, flor kau\u00e7uk, akrilat kau\u00e7uk, kloros\u00fclfonatl\u0131 polietilen, klorlu b\u00fctil kau\u00e7uk, nitril kau\u00e7uk, neopren kau\u00e7uk gibi halojen elementler, Siyano grubu, ester grubu vb. i\u00e7erir.<\/p>\n\n\n<div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full is-resized\"><img decoding=\"async\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-51.jpg\" alt=\"\" class=\"wp-image-6225\" height=\"400\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-51.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-51-300x300.jpg 300w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-51-150x150.jpg 150w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/11\/heat-resistant-rubber-51-100x100.jpg 100w\" sizes=\"(max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div>\n\n\n<h2 class=\"wp-block-heading\"><mark style=\"background-color:rgba(0, 0, 0, 0)\" class=\"has-inline-color has-vivid-cyan-blue-color\">Is\u0131ya dayan\u0131kl\u0131 kau\u00e7u\u011fun farkl\u0131 form\u00fclasyonlar\u0131<\/mark><\/h2>\n\n\n\n<p>Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uklar\u0131n farkl\u0131 form\u00fclasyonlar\u0131 farkl\u0131 s\u0131cakl\u0131klara dayanacak \u015fekilde tasarlanm\u0131\u015ft\u0131r. En yayg\u0131n form\u00fclasyonlar 350 Fahrenheit dereceye kadar olan s\u0131cakl\u0131klara dayanacak \u015fekilde tasarlanm\u0131\u015ft\u0131r. <\/p>\n\n\n\n<p>Bu form\u00fclasyon tipik olarak kau\u00e7u\u011fun conta ve ke\u00e7eler gibi aral\u0131kl\u0131 olarak y\u00fcksek \u0131s\u0131ya maruz kalaca\u011f\u0131 uygulamalarda kullan\u0131l\u0131r. <\/p>\n\n\n\n<p>Ayr\u0131ca 600 Fahrenheit dereceye kadar s\u0131cakl\u0131klara dayanabilen daha y\u00fcksek s\u0131cakl\u0131k form\u00fclasyonlar\u0131 da vard\u0131r. Bu form\u00fclasyonlar tipik olarak kau\u00e7u\u011fun kazan contalar\u0131 veya f\u0131r\u0131n contalar\u0131 gibi s\u00fcrekli olarak y\u00fcksek \u0131s\u0131ya maruz kalaca\u011f\u0131 uygulamalarda kullan\u0131l\u0131r. <\/p>\n\n\n\n<p>Kau\u00e7u\u011fun a\u015f\u0131r\u0131 s\u0131cakl\u0131klara dayanabilmesi gereken havac\u0131l\u0131k ve uzay uygulamalar\u0131 gibi \u00f6zel uygulamalar i\u00e7in daha y\u00fcksek s\u0131cakl\u0131k form\u00fclasyonlar\u0131 mevcuttur. \u00c7e\u015fitli uygulamalar\u0131n ihtiya\u00e7lar\u0131n\u0131 kar\u015f\u0131lamak i\u00e7in farkl\u0131 \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk form\u00fclasyonlar\u0131 mevcuttur.<\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full is-resized\"><img decoding=\"async\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/10\/Silicone-raw-material.jpg\" alt=\"\" class=\"wp-image-5704\" height=\"400\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/10\/Silicone-raw-material.jpg 593w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/10\/Silicone-raw-material-300x283.jpg 300w\" sizes=\"(max-width: 593px) 100vw, 593px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<h2 class=\"wp-block-heading\"><mark style=\"background-color:rgba(0, 0, 0, 0)\" class=\"has-inline-color has-vivid-cyan-blue-color\">Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk u\u00e7lar\u0131n do\u011fru kullan\u0131m\u0131<\/mark><\/h2>\n\n\n\n<p>Y\u00fcksek s\u0131cakl\u0131klara dayanabilen, g\u00fcvenilir, y\u00fcksek kaliteli, dayan\u0131kl\u0131 bir malzeme ar\u0131yorsan\u0131z, ba\u015fka yere bakman\u0131za gerek yok. <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">Is\u0131ya Dayan\u0131kl\u0131 Kau\u00e7uk<\/a>. <\/p>\n\n\n\n<p>Bu kau\u00e7uk t\u00fcr\u00fc, conta ve ke\u00e7elerde oldu\u011fu gibi y\u00fcksek s\u0131cakl\u0131klara maruz kalma olas\u0131l\u0131\u011f\u0131 olan uygulamalar i\u00e7in idealdir. Bununla birlikte, a\u015fa\u011f\u0131dakilere dikkat etmek \u00f6nemlidir <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">\u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk<\/a> yok edilemez de\u011fildir ve en iyi sonu\u00e7lar i\u00e7in do\u011fru \u015fekilde kullan\u0131lmas\u0131 gerekir. \u0130\u015fte \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7u\u011fu do\u011fru kullanmak i\u00e7in 5 ipucu.<\/p>\n\n\n\n<p><strong>1). Uygulaman\u0131z i\u00e7in do\u011fru kalitede \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk kullan\u0131n.<\/strong> Farkl\u0131 s\u0131cakl\u0131k aral\u0131klar\u0131na dayanacak \u015fekilde tasarlanm\u0131\u015f farkl\u0131 s\u0131n\u0131flar mevcuttur. \u0130htiya\u00e7lar\u0131n\u0131za uygun olan\u0131 se\u00e7ti\u011finizden emin olun.<\/p>\n\n\n\n<p><strong>2). Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk, y\u00fcksek s\u0131cakl\u0131klara maruz kald\u0131\u011f\u0131nda zamanla sertle\u015fecek ve k\u0131r\u0131lgan hale gelecektir. <\/strong>Bu, \u00e7atlamas\u0131na veya k\u0131r\u0131lmas\u0131na neden olabilir. Bunu \u00f6nlemek i\u00e7in \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk \u00fcr\u00fcnlerinizi d\u00fczenli olarak kontrol etti\u011finizden ve gerekirse de\u011fi\u015ftirdi\u011finizden emin olun.<\/p>\n\n\n\n<p><strong>3). Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk \u00fcr\u00fcnleri takarken, bunlara zarar vermemeye dikkat edin.<\/strong> Herhangi bir kesik veya y\u0131rt\u0131k \u00fcr\u00fcn\u00fc zay\u0131flatarak ar\u0131zalanmaya daha yatk\u0131n hale getirir.<\/p>\n\n\n\n<p><strong>4). Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk \u00fcr\u00fcnleri kullan\u0131rken daima \u00fcreticinin talimatlar\u0131na uyun.<\/strong> Depolama, kurulum ve bak\u0131mla ilgili bilgiler \u00fcr\u00fcn ambalaj\u0131nda veya kullan\u0131m k\u0131lavuzunda bulunabilir.<\/p>\n\n\n\n<p><strong>5). Is\u0131ya dayan\u0131kl\u0131 kau\u00e7uk kullan\u0131m\u0131 hakk\u0131nda herhangi bir sorunuz varsa, l\u00fctfen bu t\u00fcr malzemelerle \u00e7al\u0131\u015fma deneyimi olan bir profesyonele dan\u0131\u015f\u0131n. <\/strong>\u00d6zel uygulaman\u0131zda kullanman\u0131n en iyi yolu konusunda size tavsiyelerde bulunabileceklerdir.<\/p>\n\n\n\n<div class=\"wp-block-columns is-layout-flex wp-container-core-columns-is-layout-9d6595d7 wp-block-columns-is-layout-flex\">\n<div class=\"wp-block-column is-layout-flow wp-block-column-is-layout-flow\" style=\"flex-basis:100%\"><div class=\"wp-block-image\">\n<figure class=\"aligncenter size-full\"><img loading=\"lazy\" decoding=\"async\" width=\"564\" height=\"275\" src=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Material-Guide-Properties-Types-Applications.jpg\" alt=\"\" class=\"wp-image-4871\" srcset=\"https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Material-Guide-Properties-Types-Applications.jpg 564w, https:\/\/zetarmoulding.com\/wp-content\/uploads\/2022\/09\/Silicone-Rubber-Material-Guide-Properties-Types-Applications-300x146.jpg 300w\" sizes=\"auto, (max-width: 564px) 100vw, 564px\" \/><\/figure>\n<\/div><\/div>\n<\/div>\n\n\n\n<h2 class=\"wp-block-heading\"><mark style=\"background-color:rgba(0, 0, 0, 0)\" class=\"has-inline-color has-vivid-cyan-blue-color\">Sonu\u00e7<\/mark><\/h2>\n\n\n\n<p>Form\u00fclasyon tasar\u0131m\u0131 <a href=\"https:\/\/zetarmoulding.com\/tr\/\" target=\"_blank\" rel=\"noreferrer noopener\" title=\"https:\/\/zetarmoulding.com\/\">\u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk<\/a> hala a\u00e7\u0131k bir sorundur. Bununla birlikte, ara\u015ft\u0131rmac\u0131lar termal stabiliteyi ve mekanik \u00f6zellikleri iyile\u015ftirmek i\u00e7in bir dizi \u00e7\u00f6z\u00fcm \u00f6nermi\u015flerdir. <a href=\"https:\/\/zetarmoulding.com\/tr\/\" title=\"https:\/\/zetarmoulding.com\/\">\u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uklar<\/a>. Bu derleme makalenin, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7u\u011fun form\u00fclasyon tasar\u0131m\u0131 \u00fczerine gelecekteki ara\u015ft\u0131rmalar i\u00e7in baz\u0131 yararl\u0131 ayd\u0131nlatmalar sa\u011flayabilece\u011fini umuyoruz.<\/p>","protected":false},"excerpt":{"rendered":"<p>Is\u0131n\u0131n kau\u00e7uk \u00fcr\u00fcnlere zarar verebilece\u011fi bir s\u0131r de\u011fildir. Ancak kau\u00e7u\u011fu y\u00fcksek s\u0131cakl\u0131klara dayanabilecek \u015fekilde form\u00fcle etmenin yollar\u0131 oldu\u011funu biliyor muydunuz? Bu blog yaz\u0131s\u0131nda, \u0131s\u0131ya dayan\u0131kl\u0131 kau\u00e7uk form\u00fcle etmenin farkl\u0131 yollar\u0131n\u0131 ve bunlar\u0131n i\u015fletmenize nas\u0131l fayda sa\u011flayabilece\u011fini inceleyece\u011fiz. Ayr\u0131ca baz\u0131 fakt\u00f6rleri de tart\u0131\u015faca\u011f\u0131z [...]<\/p>","protected":false},"author":1,"featured_media":6223,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_seopress_robots_primary_cat":"none","_monsterinsights_skip_tracking":false,"_monsterinsights_sitenote_active":false,"_monsterinsights_sitenote_note":"","_monsterinsights_sitenote_category":0,"footnotes":""},"categories":[1],"tags":[],"class_list":["post-6204","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-uncategorized"],"_links":{"self":[{"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/posts\/6204","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/comments?post=6204"}],"version-history":[{"count":24,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/posts\/6204\/revisions"}],"predecessor-version":[{"id":6248,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/posts\/6204\/revisions\/6248"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/media\/6223"}],"wp:attachment":[{"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/media?parent=6204"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/categories?post=6204"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/zetarmoulding.com\/tr\/wp-json\/wp\/v2\/tags?post=6204"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}